VRSCSE CVO VROD rear Reactor wheel
by Editor on 07/22/22
Good from far but far from good.
After using AutoSol, a soft cloth with light pressure I was able to flatten many of the "bumps". (normally I wouldn't use that on chrome because it has an abrasive in it)
Mothers chrome polish was used next and this is the final result.
Definitely a lot better than it was but unfortunately there are some blisters in the chrome and spots where it's missing but this is as good as it gets. Only so much can be done with neglected chrome...
It will go back on the bike like this so I can ride it for the remaining season then decide if I will re-chrome it over the winter.
click here for more on this bike